| CYCLONES
/ PREHEATERS
Erosion from dust particles, thermal shock and thermal cycling
are all factors leading to the progressive wear of preheater
linings. Steel fibres increase refractory toughness to improve
performance and provide a long-term solution.
Recommendation: ME 304, ME 430
RISER
DUCTS
Riser duct refractory deteriorates due to clinker dust
penetration and/or impact from high-pressure water or mechanical
cleaning (to remove the build up of Sulphates). Steel fibre
reinforcement lessens refractory damage and lengthens refractory
lifetime, saving maintenance and costs.
Recommendation: ME 310, ME 446